IINTRODUCTION
Stone Mastic asphalt (SMA), otherwise known as Stone
Matrix Asphalt / Split Mastic Asphalt, was developed in Germany in the mid of
1960's and it has spread throughout Europe and across the world in 1980's and
1990's respectively. The excellent performances include resistant to mechanical
and temperature deformation, cracking, and particularly rutting, resistant to
weathering actions such as aging and low temperature cracking. Durability is
excellent even under slow moving heavy traffic. The textured surface increases
skid resistance and provides environmental and driving comfort by reduced noise
level, and improved visibility in rainy days.
SMA provides a
deformation resistant, durable, surfacing material, suitable for heavily
trafficked roads. SMA has found use in Europe, Australia
and the United States
as a durable asphalt surfacing option for residential streets and highways. SMA
has a high coarse aggregate content that interlocks to form a stone skeleton
that resist permanent deformation. The stone skeleton is filled with mastic of
bitumen and filler to which fibres are added to provide adequate stability of
bitumen and to prevent drainage of binder during transport and placement.
Typical SMA composition consists of 70−80% coarse aggregate, 8−12% filler,
6.0−7.0% binder, and 0.3 per cent fibre. The deformation resistant capacity of
SMA stems from a coarse stone skeleton providing more stone-on-stone contact
than with conventional dense graded asphalt (DGA) mixes. Improved binder
durability is a result of higher bitumen content, a thicker bitumen film and,
lower air voids content. This high bitumen content also improves of
flexibility. Addition of a small quantity of cellulose or mineral fibre
prevents drainage of bitumen during transport and placement. The essential
features, which are the coarse aggregate skeleton and mastic composition, and
the consequent surface texture and mixture stability, are largely determined by
the selection of aggregate grading and the type and proportion of filler and
binder.
SMA is characterized by a stone-on-stone structure. SMA uses a high
proportion of larger stones or aggregate that contacts each other. This
skeleton of larger stones resists heavy loads by transmitting them to the
pavement below. If the under laying pavement is sufficiently strong then the
SMA will resist the heavier loads effectively. (A surfacing cannot compensate
for a weak pavement).
3. PERFORMANCE CHARACTERISTICS OF SMA
The development of modern pavement
technology is needed to accelerate significant improvement of pavement quality
of highways, airport runways and urban roads.
SMA meets the following demands upon
an asphalt pavement:
· Good stability at high temperatures
· Good flexibility at low temperatures
· High wearing resistance
· High adhesive capacity between the stone granules and the
bitumen
· A mix with no tendency to separate
· Good skid resistance
· Reduced water spray
· Lower traffic noise
Good stability at high temperatures
SMA mix has a self-supporting stone
skeleton of crushed high quality coarse aggregate, which provides an increase
in internal friction and shear resistance and hence its extremely high stability.
Good flexibility at low temperatures
SMA mix has a binder rich mastic
mortar which has superior properties over dense graded asphalt in resisting
thermal cracking.
High wearing resistance
SMA mix has low air voids, which make
the mix practically impermeable, and provide satisfactory ageing resistance,
moisture susceptibility and durability.
High adhesive capacity between the
stone granules and the bitumen
With the increase of the amount of
filler, cellulose fibres are added as stabiliser. The three dimensional
structure of cellulose fibre assists the bitumen to maintain a high viscosity,
thickens the bituminous film and improves the bitumen/aggregate adhesion.
A mix with no tendency to separate
An efficient stabilisation of the mastic in order to prevent its segregation
from the coarse particles.
Good skid resistance
Because of the macro-texture of the
road surface and the use of coarse aggregates with a high Polished Stone Value,
SMA pavement achieves a better level of skid resistance.
Reduced water spray
Because of its greater texture depth,
there is less water spray, and at night there is fewer glares reflected from
the road surface and better visibility of road markings.
Lower traffic noise
SMA road surfaces generally offer
lower levels of noise due to the texture properties.
4. COMPOSITION OF SMA
Stone Mastic Asphalt is characterised
by its high stone content which forms a gap-graded skeleton-like stone
structure. The voids of the structural matrix are filled with high viscosity
bituminous mastic. The high stone content of at least 70% ensures
stone-on-stone contact after compaction. The required degree of mastic
stiffness is achieved through the addition of crushed sand.
SMA mixes have a bitumen content of
minimum 6.5%. The bitumen in the gap-graded mix is stabilised during the mixing
process, intermediate storage, transportation, surfacing and compaction through
the addition of cellulose fibre stabilising additive.
Addition of cellulose fibre does not
chemically modify bitumen, but rather enhances physical property of the
finished product by allowing the use of higher bitumen contents. It tends to
thicken or bulk the bitumen so that it does not run off the aggregate prior to
compaction. The content of cellulose fibre is 0.3% by weight of mixture. If the
technological requirements of SMA are fully met, good results can be obtained
by just using standard bitumen and a cellulose fibre drainage inhibitor.
4.1 Materials Used
1. Coarse and fine aggregate
2. Bitumen
3. Fibre
4. Filler
4.1.1 Coarse and fine aggregate
The aggregates are crushed by using
jaw pressure to get different size of aggregates varying from 16 mm to 75
micron. The coarse aggregate must be hard, durable, and roughly cubical in
shape when crushed. Qualities of aggregates were check through various tests
like Impact Value Test, Crushing Value Test, Los Angel’s Abrasion Value Test,
Flakiness and Elongation Index Test.
4.1.2 Bitumen
Bitumen act as a binder in SMA
mix. Different grade of bitumen are used in different mix like hot-mix or
gap-graded mix or dense-graded mix. For preparation of SMA mix we used 60/70
bitumen.
4.1.3 Fibre
Fibres are used as stabiliser in SMA
mix. Fibres help to increase the strength and stability and decrease the drain
down in SMA mix. There are different types of fibres are used in SMA mix like
cellulose fibre, polymer fibre, natural fibre and mineral fibre.
4.1.4 Filler
Filler is used in SMA mix for better
binding of materials. Rock dust, slag dust, hydrated lime, hydraulic cement,
fly ash, mineral filler and cement are used as filler in SMA mix, also we can
use the fine aggregate below 75 micron as filler.
5. ADVANTAGES
· 20-30% increase in pavement life over conventional pavements
· Good aggregate interlock
· Low permeability
· Improve in skid resistance due to the high percentage of
fractured aggregate to motoring public particularly on wet pavement.
· Surface texture characteristic may reduce sound from the tyre
and pavement contact as well as water spray and glare.
· Strength and stiffness derived from binder and aggregate
structure
· Relatively high binder contents provide good Durability
· Durability (longer in-service life) of SMA should be equal to,
or greater than, DGA and significantly greater than OGA.
· It provides a textured, durable and rut resistant wearing
course.
· Surface texture characteristics are similar to OGA, so noise generated
is lower than DGA but slightly higher than OGA.
· It can be produced and compacted with the same plant and
equipment as for normal hot mix DGA using procedural modifications.
· SMA can be used on heavily trafficked roads where good
deformation resistance is required.
· Surfacing may reduce reflective cracking from underlying cracked
pavements due to its flexible mastic.
· At the end of its service life it is 100% recyclable.
6. DISADVANTAGES
· SMA mix requires higher mixing temperature.
· Potential construction problem with SMA mixtures are drainage
and bleeding.
· Storage and placement temperatures cannot be lowered to control
drainage and bleeding problem due to the difficulty in obtaining the required
compacted.
· Increased material cost associated with high bitumen and filler
content.
· Increased mixing time and time taken to add extra filler may
result in reduced productivity.
· Possible delays in openings (the road) as SMA should be cooled
to 40°c to prevent early flushing of the binder to the surface.
· Needs more carefully monitoring the composition at the mixing
plant.
· Moisture seeping from the SMA surface for long periods after
rain.
· White fines on the surface of the pavements.
· Premature rutting
· Stripping of asphalt layers below the SMA surfacing.
· Potholing
7. APPLICATIONS
Stone Mastic Asphalt has proved
superior on heavily trafficked roads and industrial applications:
· with high lorry frequency
· intense wheel tracking
· at traffic lights
· at intersections
· on highways
· on gradients
· on bridges
· in bus lanes
· at bus-stops
· in car parks
· in harbours
· on airport runways
· on un/loading areas